Re: T&T: bottom paint / personal preference

C
CaribouMike55@aol.com
Thu, Apr 14, 2005 5:58 PM

In my own personal observations, it's going to be hard to beat Woolsey
Neptune, (votes not yet in for Neptune II) My last application has gone 4 years, in
SC, with nothing but minor fouling
A friend did an exceptional job, 12 mils of Copperpoxy, and the next time he
passes through, we will update his results.

A friend gave me some Trinidad SR to use on my RIB. It has stuck well on both
fibergas and Hypalon tubes. One year and counting - two coats.
John DeLotto

In my own personal observations, it's going to be hard to beat Woolsey Neptune, (votes not yet in for Neptune II) My last application has gone 4 years, in SC, with nothing but minor fouling A friend did an exceptional job, 12 mils of Copperpoxy, and the next time he passes through, we will update his results. A friend gave me some Trinidad SR to use on my RIB. It has stuck well on both fibergas and Hypalon tubes. One year and counting - two coats. John DeLotto